Home›Insights›Technology Notes›Antioxidant Masterbatch
Technology Note · November 2026

Antioxidant Masterbatch: Protecting Recycled PE and PP

Every time polyethylene or polypropylene is melted, it loses some of the antioxidant that protects it. Recycled material has already been through that cycle at least once, so it often arrives with too little protection left for another life.

Polymer masterbatch pellets for recycled plastics

Heat, shear and oxygen in the extruder create free radicals in the polymer. Left unchecked, they start a chain reaction that breaks or links the polymer chains. Polypropylene mostly suffers chain scission: the melt flow rises, the material gets weaker and parts turn brittle. Polyethylene tends to crosslink, which raises viscosity and causes gels, specks and poor film appearance. Both lose colour, usually turning yellow.

Virgin resin is supplied with a stabiliser package to protect it through its first processing and its service life. That package is consumed along the way. By the time packaging or parts are collected, washed and reprocessed, much of it is gone, and the new heat history of recycling uses up more. Recyclate also contains residues, inks and traces of metals that can speed up oxidation.

Antioxidants work as a team. Primary antioxidants, usually hindered phenols, trap free radicals and give long-term heat stability. Secondary antioxidants, usually phosphites, break down hydroperoxides during processing, protecting the melt and the colour. Most stabiliser packages for recycling combine the two, because processing stability and long-term stability are different problems.

An antioxidant masterbatch is the simplest way to put that protection back. Dosed through the existing feeder at the recycling extruder or at the converter, it restores processing stability, keeps the melt flow closer to specification and reduces gels and discolouration. It also helps the recycled material survive the next melt, which matters as more products are designed to be recycled more than once.

How to stabilise recycled PE and PP well.

Measure first

Check melt flow, colour and, where possible, oxidation induction time (OIT) on the incoming recyclate.

Add it early

Antioxidant works best when dosed at the first melt, before damage is done, rather than at the end.

Match the polymer

PP is more sensitive to chain scission than PE and usually needs more protection.

Treat the other faults

Moisture and odour are separate problems: use a desiccant and an odour absorber alongside.

Compare the result on the properties that matter to your customer: melt flow stability over several passes, colour, gel count in film and impact strength in moulded parts. A small trial at two or three dose levels shows where the benefit levels off, so you do not pay for more additive than you need.

Aviura's AOX antioxidant masterbatch protects PE and PP through processing and recycling, and our UVX grade combines antioxidant and UV protection for outdoor products. Tell us the source of your recyclate, your process and the problems you see, and we will recommend a starting dose for a trial.

Recycled polymer has spent part of its protection already. Put it back before the next melt, not after.

See polymer protection grades

Related reading

← Back to Technology Notes