Application · Packaging film

Slip and antiblock masterbatch forblown and cast packaging film.

Film that opens cleanly, does not stick on the roll and runs fast on form-fill-seal and bag-making lines.

Polyethylene film is naturally tacky. Layers stick together on the roll (blocking), bags are hard to open, and film drags over forming collars and sealing jaws, which slows packing lines and causes jams.

Antiblock adds fine mineral particles that roughen the film surface very slightly, so layers do not cling. Slip additives migrate to the surface and lower the coefficient of friction (COF), so film slides over metal and over itself. Most packaging film needs both, and a combined slip-antiblock grade puts them in one dose.

Slip keeps migrating after extrusion, so COF changes as the film ages, and it is also affected by temperature, film thickness and the resin. We test COF, migration and ageing so the film arrives at your customer's line with the friction they specified.

Request a sampleRequest a quote
Grades

Grades for packaging film

SABSlip + antiblock

Film opening and machinability in one dose.

PE / LLDPE · Flexible packaging

SLPSlip

Lowers the coefficient of friction.

PE / LLDPE · Flexible packaging film

ABKAntiblock

Reduces film blocking.

PE / LLDPE · Packaging and industrial film

PPAPolymer processing aid

Removes melt fracture and cuts die build-up.

PE / LLDPE · Blown film and extrusion

ASTAntistatic

Reduces static charge and dust pick-up.

PE / PP · Packaging and industrial plastics

AOXAntioxidant

Thermal-oxidation protection, including in recycling.

PE / PP · Film, extrusion, injection and recycling

What controls slip and blocking in film.

Target COF

Agree the target COF with your customer: it sets the slip dose.

Ageing

Slip takes time to migrate, so measure COF after ageing, not straight off the line.

Haze

Antiblock affects clarity, so balance blocking force against haze for clear packs.

Printing and lamination

Too much slip can affect print and lamination adhesion: tell us how the film is converted.

Questions

Frequently asked questions

What is the difference between slip and antiblock?

Antiblock stops film layers sticking to each other, using fine mineral particles on the surface. Slip lowers friction between the film and other surfaces. They solve different problems and are often used together.

Why does film COF change after production?

Slip additives keep migrating to the surface for some time after extrusion, so COF usually falls as the film ages. Storage temperature and film thickness change the speed of that migration.

Are your slip and antiblock grades suitable for food packaging?

Food-contact declarations (EU 10/2011, US FDA 21 CFR) are available where the formulation qualifies. Tell us the end use and we will confirm the documents for the grade.

How do I get a sample?

Send us your polymer, process and the problem you want to solve. We recommend a grade and starting let-down, then ship a 1 kg lab sample, 5 kg pilot sample or 25 kg line trial with TDS, SDS and batch COA.

Further reading

Sampling

From brief to first order.

Masterbatch has to prove itself on your extruder, not ours. This is the route every new grade takes.

  1. 1

    Send your brief

    Polymer, process, the problem to solve, and your current product if you have one.

  2. 2

    We recommend

    A grade and a starting let-down for your line, shared with you shortly.

  3. 3

    Sample ships

    A 1 kg lab sample, 5 kg pilot sample or 25 kg line trial, with TDS, SDS and batch COA.

  4. 4

    You trial

    We review the results with your team and adjust dosage or formulation.

  5. 5

    Quote and order

    Price, MOQ and lead time fixed against the approved grade.